dc.creatorLordelo, Rodrigo Seixas Dourado-
dc.creator.Latteshttp://lattes.cnpq.br/9853239695099717por
dc.contributor.advisor1Moura, Washington Almeida-
dc.contributor.advisor1Lattes14678349553por
dc.date.accessioned2018-09-10T20:23:00Z-
dc.date.issued2018-07-16-
dc.identifier.citationLORDELO, Rodrigo Seixas Dourado. Avaliação da utilização de resíduo de vidro de garrafas na produção de argamassa. 2018. 102 f. Dissertação (Mestrado em Engenharia Civil e Ambiental)- Universidade Estadual de Feira de Santana, Feira de Santana, 2018.por
dc.identifier.urihttp://tede2.uefs.br:8080/handle/tede/700-
dc.description.resumoA utilização de resíduos incorporados à materiais de construção vem sendo apontada como uma alternativa para destinação mais adequada dos resíduos sólidos. Dentre os resíduos gerados no Brasil, estão os de vidro. Menos da metade das embalagens de vidro produzidas no Brasil são recicladas. No presente trabalho foi avaliado a influência da utilização de resíduo de vidro de garrafas de cor marrom, triturado, como substituto parcial do agregado miúdo natural, na produção de argamassas. Os teores de substituição avaliados foram de 10, 20 e 30%, em massa, além da argamassa de referência (sem resíduo). Foram analisadas propriedades das argamassas no estado fresco (trabalhabilidade, massa específica e teor de ar incorporado) e no estado endurecido (resistência à tração na flexão, resistência à compressão, absorção de água, índice de vazios, massa específica e reatividade álcali-sílica). Os resultados dos ensaios indicaram que o uso de resíduo de vidro de garrafa, em substituição ao agregado natural, não alterou a fluidez das argamassas, mas diminuiu a densidade e aumentou o teor de ar incorporado. A incorporação do resíduo proporcionou aumento nas resistências à tração na flexão e à compressão, comparado à argamassa de referência. Com relação à possível reatividade álcali-sílica, verificou-se que as argamassas com o resíduo de vidro de garrafa não excederam o limite de expansão estabelecido conforme a NBR 15577-4 (ABNT, 2009). Com base nos resultados concluiu-se que é possível utilizar até 30% de resíduo de garrafa de vidro de cor marrom, em substituição ao agregado natural.por
dc.description.abstractThe use of waste incorporated in building materials has been pointed out as an alternative for more adequate disposal of solid waste. Among the wastes generated in Brazil, are the glass. Less than half of the glass bottles produced in Brazil are recycled. In the present work the influence of the use of waste glass of brown bottles, crushed, as partial substitute of the natural sand, in the production of mortars was evaluated. The substitution contents evaluated were 10, 20 and 30%, by mass, in addition to the reference mortar (without waste glass). The properties of the mortars in the fresh state were evaluated (workability, specific mass and incorporated air content) and also in the hardened state (flexural tensile strength, compressive strength, water absorption, void index, specific mass and alkali-silica reactivity). The results of the tests indicated that the use of waste glass bottles, replacing the natural aggregate, did not alter the fluidity of the mortars, but decreased the density and increased the content of incorporated air. The incorporation of the waste provided an increase in the tensile strengths in flexion and compression, in relation to the reference mortar. With respect to the possible alkali-silica reactivity, it was verified that the mortars with the waste glass bottle did not exceed the expansion limit established in accordance with NBR 15577-4 (ABNT, 2009). Based on the results it was concluded that it is possible to use up to 30% of waste glass of brown bottles, replacing the natural sand.eng
dc.description.provenanceSubmitted by Ricardo Cedraz Duque Moliterno (ricardo.moliterno@uefs.br) on 2018-09-10T20:23:00Z No. of bitstreams: 1 AVALIAÇÃO DA UTILIZAÇÃO DE RESÍDUO DE VIDRO DE GARRAFAS NA PRODUÇÃO DE ARGAMASSA.pdf: 2101422 bytes, checksum: 3e30e4c6ad0b0e448d0f28282d5385fa (MD5)eng
dc.description.provenanceMade available in DSpace on 2018-09-10T20:23:00Z (GMT). No. of bitstreams: 1 AVALIAÇÃO DA UTILIZAÇÃO DE RESÍDUO DE VIDRO DE GARRAFAS NA PRODUÇÃO DE ARGAMASSA.pdf: 2101422 bytes, checksum: 3e30e4c6ad0b0e448d0f28282d5385fa (MD5) Previous issue date: 2018-07-16eng
dc.formatapplication/pdf*
dc.languageporpor
dc.publisherUniversidade Estadual de Feira de Santanapor
dc.publisher.departmentDEPARTAMENTO DE CIÊNCIAS HUMANAS E FILOSOFIApor
dc.publisher.countryBrasilpor
dc.publisher.initialsUEFSpor
dc.publisher.programMestrado em Engenharia Civil e Ambientalpor
dc.rightsAcesso Abertopor
dc.subjectArgamassapor
dc.subjectResíduo de vidropor
dc.subjectPropriedades das argamassaspor
dc.subjectReciclagempor
dc.subjectMortareng
dc.subjectGlass wasteeng
dc.subjectMortar propertieseng
dc.subjectRecycling.eng
dc.subject.cnpqENGENHARIA CIVIL::CONSTRUCAO CIVILpor
dc.titleAvaliação da utilização de residuo de vidro de garrafas na produção de argamassapor
dc.typeDissertaçãopor
Appears in Collections:Coleção UEFS

Files in This Item:
File Description SizeFormat 
AVALIAÇÃO DA UTILIZAÇÃO DE RESÍDUO DE VIDRO DE GARRAFAS NA PRODUÇÃO DE ARGAMASSA.pdfArquivo em texto completo.2.05 MBAdobe PDFDownload/Open Preview


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.